Erosion Corrosion

Tuberculation and Erosion Corrosion

Tuberculation and erosion corrosion of washing machine water tap

Tuberculation and erosion corrosion of washing machine water tap

The development or formation of small mounds of corrosion products or tuberculation on the inside of steel pipe can roughen the inside of the pipe, increasing its resistance to water flow and the possibility of erosion corrosion.


 