Conclusions
- The corrosion-related performance of subcomponents can be analyzed
explicitly in terms of the CBDA/LAM method. This approach integrates all the
important contributions from corrosion.
- The CBDA/LAM method provides frameworks within which mathematical
expressions can be utilized to quantify corrosion at specific LAis.
- This CBDA/LAM approach provides a basis for the explicit considerations of
corrosion in such a way that they can become part of the design record and
are not omitted in the apparent complexity of corrosion-related phenomena.
- The CBDA/LAM approach provides an approach that can be understood and
utilized by both materials and design organizations..

Lifetime Prediction, Roger W. Staehle,
Adjunct Professor, Department of Chemical Engineering and Materials Science,
University of Minnesota, Staehle
Consulting Co.