Pack rust is a form a localized corrosion typical of steel components that develop a crevice into an open atmospheric environment. This expression is often used in relation to bridge inspection to describe built-up members of steel bridges which are showing signs of rust packing between steel plates.

Courtesy: Termarust (Wayne A. Senick)