Equivalent circuit models the AS4/3501-6, FM300, Al core honeycomb composite. The circuit should be able to model similarly constructed materials by varying the values of the individual circuit elements.
Figure 16
In-Situ Sensor to Detect Moisture Intrusion and Degradation of Coatings, Composites, and Adhesive Bonds, G.D. Davis, C.M. Dacres, and L.A. Krebs, DACCO SCI Inc.