Figure 1 A depiction of the degradation process (after Hoeppner-1971, 1986)
Review of Pitting Corrosion Fatigue Models, D.W. Hoeppner, V. Chandrasekaran, and A.M.H. Taylor, University of Utah and FASIDE International Inc.