Current density profile duringDC interference

Figure 17 Current density profile along the pipeline for a train at position 1 in Figure 13.


Study and Evaluation of Stray Current Influences on Cathodic Protection Systems of Buried Pipelines, L. Bortels, ELSYCA - Kranenberg 6 - 1731 - BELGIUM, ELSYCA